Zinc • Transition Metal

Primary XPS region: Zn2p
Overlapping regions: O KLL, V LMM
Binding energies of common chemical states:

Chemical stateBinding energy Zn2p3/2
Zn metal1,021.7 eV
ZnO~1,022 eV

Oxide charge referenced to adventitious C1s peak at 284.8eV.

 

Experimental Information

  • There are small binding energy shifts of some compounds compared to zinc metal.
    • Chemical state differentiation can be difficult with XPS only.
    • Collect principal Zn LMM peak as well as Zn2p.
      • There are bigger chemical shifts observed for Zn LMM compared to Zn2p.

 

Interpretation of XPS spectra

  • Zn2p peak has significantly split spin-orbit components (Δmetal=23eV).
  • ZnO has an unusual O1s spectrum with two peaks, possibly indicating either Zn(OH)2, ZnCO3,
    or oxygen vacancies.
  • Zinc shows only a small binding energy shift in the Zn2p3/2 region (1021eV - 1023eV, modal value).
    • Peak width may broaden in the presence of more than one Zn species.
  • Zn2p peaks often accompanied by Auger peak at Kinetic Energy ~990eV.
    • If zinc is buried (under carbon, for example), Zn Auger peak may be observed even if Zn2p is not (due to difference in electron kinetic energy).
    • Similarly, Zn3p (very high kinetic energy) may be observed even if Zn2p is not.
  • Use X-ray induced Zn LMM Auger peaks, which have a larger shift with chemical state.
    • Use Wagner plot to help assign chemistry.

 

Zn LMM Spectra Zinc Metal Compounds

General comments

  • There have been concerns about mobility of zinc in alloys and vapor pressure with concern about introducing zinc into a high-vacuum environment.
    • In practice, this is not a major concern if the sample is not heated in vacuum.

 

Element Crystal Hex

About this element

Symbol: Zn
Date of discovery: 1746
Name origin: German zink
Appearance: blue-white
Discoverer: Andreas Marggraf
Obtained from: zinc blende, calamine

Melting point: 692 K
Boiling point: 1180 K
Density[kg/m3]: 7140
Molar volume: 9.16 × 10-6 m3/mol
Protons/Electrons: 30
Neutrons: 35
Shell structure: 2,8,18,2
Electron configuration: [Ar]3d104s2
Oxidation state: 2,3
Crystal structure: hexagonal

Zinc alloys have been used for centuries; although, A. Marggraf is credited for the first isolation of zinc from the charcoal reduction of calamine in 1746. This bluish-white metal is brittle at ambient temperatures, but becomes malleable between 110–150°C. It is an essential element in the growth of plants and animals, and altered biological concentrations of zinc can lead to severe health problems. Zinc’s principle use is to galvanize iron and steel, preventing corrosion. It is also used to form numerous metal alloys such as brass, bronze, and aluminum solder. Zinc oxide is used in plastics, cosmetics, and wallpaper, while zinc sulfide is employed in luminescent dials, TV screens, and fluorescent lights.

Zinc • Transition Metal

Products

Nexsa G2 XPS

  • Micro-focus X-ray sources
  • Unique multi-technique options
  • Dual-mode ion source for monoatomic & cluster ion depth profiling
Style Sheet for Instrument Cards Original

K-Alpha XPS

  • High resolution XPS
  • Fast, efficient, automated workflow
  • Ion source for depth profiling

ESCALAB QXi XPS

  • High spectral resolution
  • Multi-technique surface analysis
  • Extensive sample preparation and expansion options

Contact us

Style Sheet for Global Design System
Style Sheet for Komodo Tabs
Style Sheet to change H3 to p with em-h3-header class
Style Sheet to change H2 style to p with em-h2-header class
Style Sheet for Products Table Specifications
Style Sheet for Global Design System
Style Sheet for Komodo Tabs
Style Sheet to change H3 to p with em-h3-header class
Style Sheet to change H2 style to p with em-h2-header class
Style Sheet for Products Table Specifications
Fix for left nav
Style Sheet for Support and Service footer
Style Sheet for Fonts
Style Sheet for Cards

Electron microscopy services for
the materials science

To ensure optimal system performance, we provide you access to a world-class network of field service experts, technical support, and certified spare parts.